Try using photosensitive polyimide. Pavan On Mon, Aug 3, 2009 at 12:17 PM, DongJuan Xiwrote: > polyimide > > On Sun, Aug 2, 2009 at 6:01 PM, Reza Rashidi wrote: > > Hi everyone, > > > > Does anybody know which photoresist with a thickness of 10 um (other than > SU-8) doesn't melt up to 180 C? How good is SPR? I want to pattern a > photoresist layer on si which permanently stays in the middle of device and > acts as a spacer between two chips. However, changing mechanical properties > of the photoresist with temperature doesn't matter. The device works at high > temperature. > > > > Any suggestions would be highly appreciated. > > > > Thanks, > > Reza -- Pavan Samudrala