durusmail: mems-talk: thermally curable glue
thermally curable glue
2009-08-11
2009-08-11
2009-08-13
2009-08-14
2009-08-14
2009-08-17
2009-08-18
2009-08-18
thermally curable glue
Kuijpers, Peter
2009-08-14
Hello,

This is rather thick for spincoating, but I maybe you can use a dry film
 In the past we used a dry film from FujiFilm

Best regards,

Peter Kuijpers
MiPlaza Technology Laboratories
Philips Research Europe
High Tech Campus 04
Postbox HTC-4-1
5656 AE Eindhoven
The Netherlands
Tel.: +31 402743667
        +31 612507027
Email: p.e.m.kuijpers@philips.com

-----Original Message-----
From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On
Behalf Of Fei Wang
Sent: Friday 14 August 2009 11:23
To: General MEMS discussion
Subject: Re: [mems-talk] thermally curable glue

Hi all,

I am also trying to find a good way to do wafer bonding with thick
layer like 60um. Is that possible for SU-8 or BCB?