durusmail: mems-talk: thermally curable glue
thermally curable glue
2009-08-11
2009-08-11
2009-08-13
2009-08-14
2009-08-14
2009-08-17
2009-08-18
2009-08-18
thermally curable glue
Roger Shile
2009-08-17
I'm curious as to exactly what kind of Fujifilm you used for bonding.  I
only see photographic products on the Fujifilm website.

Roger Shile

-----Original Message-----
From: mems-talk-bounces@memsnet.org
[mailto:mems-talk-bounces@memsnet.org] On Behalf Of Kuijpers, Peter
Sent: Friday, August 14, 2009 5:49 AM
To: General MEMS discussion
Subject: Re: [mems-talk] thermally curable glue

Hello,

This is rather thick for spincoating, but I maybe you can use a dry film
 In the past we used a dry film from FujiFilm

Best regards,

Peter Kuijpers