Gold peel off with PMMA mask
2009-08-18
Gold peel off with PMMA mask
luhaorice
2009-08-19
Thanks for your reply.  We didn't open windows near every fine lines.
We also have peel off problem at areas far away (hundreds of microns)
from the windows (rectangle about 1um by 10um).

Thanks,
Hao

Ruiz, Marcos Daniel (SENCOE) wrote:
> Is it possible that the PMMA pattern was undercut in the fine areas?
>
> Dan