2009-08-20
Hi everybody,

I have a 600nm VO2 thin film made on an Si wafer. I need to pattern it with a
traditional photolithography method. But I don't know the etching recipe for VO2
film. Any suggestions
on a dry etch or wet etch are really appreciated. Thanks.

JQ Gu