70,000 Angstroms of Indium for a flip chip process. 130,000 Angstroms of standard positive resist and image reversal. I am on vacation this week. I will send technical papers next week. Bill Moffat ________________________________ From: mems-talk-bounces@memsnet.org on behalf of Chih-Chieh Cheng Sent: Tue 8/25/2009 12:51 PM To: mems-talk@memsnet.org Subject: [mems-talk] Lift-off 8000 A gold using PR 5214 Hello everyone, As title, has anyone ever tried lift-off 8000 A gold (or any other metal) using PR 5214? The thickness of gold is relatively thick so I am wondering it may not work perfectly. Thanks for your time. CC