durusmail: mems-talk: Re: SU-8
Re: SU-8
Re: SU-8
Xing Yang
1998-10-22
I believe Prof. Sharpe from Johns Hopkins University has
a paper on the testing of SU-8 mechanical properties.
Although only ultimate strength was given in that paper,
other properties might be reported in more recent papers.

Hope this helps.

Xing

-------------------------------------------------
Xing Yang, Ph.D.          3906 Trust Way
Senior Research Engineer  Hayward, CA 94545-3716
ACLARA BioSciences, Inc.  (510)293-1855 ext. 136
http://www.aclara.com     (510)293-1858 (Fax)
-------------------------------------------------

> Dear all,
>
> I am currently working on SU-8, negative photoresist. I have been looking
> for the mechanical properties (like young modulus, hardness, density,
> modulus of elasticity etc) of this material. I would like to know the
> mechanical properties of this material under any condition. I would greatly
> appreciate your help. Thank you.
>
> Best regards
> Andrew Ho
> Nanyang Technological University
>
>


reply