Hi, Ion Mill does not have any selectivity, it etches at the sputter rate of the material, everything etches, organics are slower than metals but most metals are real close to each other for sputter rate. Rick -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Deepasree Konduparthi Sent: Monday, September 14, 2009 12:36 PM To: General MEMS discussion Subject: [mems-talk] Pt Ion Milling Hi all: I am looking for Ion milling recipes/vendors for etching Pt with Au as a mask. I would prefer it to have selectivity to Ti, but can manage if it has etch selectivity to Silicon. I tried wetching pt and it is a mess and would prefer ion milling. I would appreciate your response. Thanks Deepa