durusmail: mems-talk: Pt Ion Milling
Pt Ion Milling
Pt Ion Milling
Ad Hall
2009-09-15
Here are some ion mill selectivity numbers for Au:Ti:Si

1.76 : 0.38 : 0.39

It will depend on your Accelerator Voltage but this is a good reference.

Ad

-----Original Message-----
From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org]
On Behalf Of Ruiz, Marcos Daniel (SENCOE)
Sent: Tuesday, September 15, 2009 1:24 PM
To: General MEMS discussion; deepasree.k@gmail.com
Subject: Re: [mems-talk] Pt Ion Milling

This has also been my experience.

-----Original Message-----
From: mems-talk-bounces@memsnet.org
[mailto:mems-talk-bounces@memsnet.org] On Behalf Of Morrison, Richard
H., Jr.
Sent: Tuesday, September 15, 2009 11:49 AM
To: deepasree.k@gmail.com; General MEMS discussion
Subject: Re: [mems-talk] Pt Ion Milling

Hi,

Ion Mill does not have any selectivity, it etches at the sputter rate of
the material, everything etches, organics are slower than metals but
most metals are real close to each other for sputter rate.

Rick
reply