Hi all, I've been trying to flow in fluorescence die (Rhodamine) in a PDMS microfluidic channel to do some flow characterizations. The problem is, the vicinity of the pdms channel became bright as well after about 5 minutes. It almost seemed like that the fluoresent die was diffused into the pdms. Is there a way to solve this problem? Thanks! TJ