Hi, I'm looking for a transparent layer that can protect my Al, polysilicon and nitride patterns from BOE/HF dip for 200-300minutes. There are three strict requirements: (1) The layer can withstand BOE/HF dip for 200-300minutes (2) The adhesion of the layer to its underlying Al, Polysilicon and nitride patterns is strong enough so that it will not be peeled off by BOE/HF dip. (3) The layer is easily stripped by ite remover without damaging the Al, Polysilicon and nitride patterns. I have tried SU8. It is good in (1), but bad in (2) and (3). Any suggestions will be appriciated. Thanks, Yu Wang