Electroplating question
lin yu
2009-10-14
Rick,

If I deposit a thin layer of metal on high doped Si (but the metals
are not connected together),
can I use Si as the conductive layer for electroplating?  Will this work?

Thanks,
Lin

On Wed, Oct 14, 2009 at 6:51 AM, Morrison, Richard H., Jr.
 wrote:
> In general you cannot electroplate to Silicon you need a seed for the
> metal to plate to.
>
> Rick