durusmail: mems-talk: RIE etching iron/iron oxide
RIE etching iron/iron oxide
2009-10-26
2009-10-27
2009-10-28
RIE etching iron/iron oxide
Xiaoning Wang
2009-10-26
Hello MEMS-Talk,

Is it possible to etch iron or iron oxide thin film using RIE?  What kind of
recipe should I use? I've been searching the literature but didn't come up
with anything.  Does anyone have an idea on this?

Thanks a lot!

--
Xiaoning Wang (Travis)
Graduate Student
Mechanical Engineering
Boston University
reply