Hi all, I had formed porous membrane using HF :Propane (1:1) and done electrochemical etching for duration of 10 minutes by passing 10mA/cm2 current density. However, the porosity observed in SEM pic is not good. I need suggestions on improving the electrochemical etching. regards rahul