Tungsten is not difficult to sputter at all. Usually though, what is sputtered is Ti/W with Ti being 10%, though whether by weight or atom percentage I don't remember. Ed -----Original Message----- From: mems-talk-bounces@memsnet.org [mailto:mems-talk-bounces@memsnet.org] On Behalf Of Jauniskis, Linas Sent: Monday, November 16, 2009 7:59 AM To: mems-talk@memsnet.org Subject: [mems-talk] Tungsten deposition, e-beam, sputter Hi, While I see e-beam as a recommended technique for depositing tungsten thin film, I have not been able to find a reference for what type of crucible to use. Could someone suggest crucible type? Any other particulars about e-beam of tungsten one should be aware of? Am also considering sputtering. Is tungsten particularly difficult to sputter, as compared to say titanium? Thank you, Linas.