I deposit using E-Beam and pre-expose bake at 90 deg C for 60 seconds typically. I doubt the E-beam is heating the PR, that would be a tricky issue, I don't think I can move the sample any further from the gun. On Tue, Dec 1, 2009 at 11:15 AM,wrote: > In order to determine the problem I like to know do you sputter the > materials or E beam, and are you confident the PR does not exceed the temp > were lift of becomes problematic. > > Walter@elume.com