Hi, Thanks for all your answers. I guess it could be difficult to get the whole parameters at the same time: we need to annneal some films at moderate temp. (between 80 and 200°C) under vacuum (about 10-1, 10-2 mbar) but i need also to anneal at high temperature (about 700°C) under gas flow (mainly N2). I just need to have an idea of the price in order to ask for some money .... but it is quite urgent. Thanks Regards, Alex > Need more information. What size oven, what vacuum level, what > temperature? Bill Moffat > -- Alexandre BOE Post-doctoral researcher UCL - EMIC Bat. Maxwell, b.207 Place du Levant, 3 B-1348 Louvain-la-neuve Belgium Tel. +32 10 478 106 Fax. +32 10 478 705 alexandre.boe@uclouvain.be