durusmail: mems-talk: Does petrol swell or etch PDMS?
Does petrol swell or etch PDMS?
2010-01-04
2010-01-04
Does petrol swell or etch PDMS?
Rashid, Mamun
2010-01-04
Hello,

Petrol deformed microfluidic PDMS structure, it also depends on the UV cured
PDMS substrate condition.


Mamun Rashid
Research Assistant
Centre for Nano & Microsystems
University of Teesside
TS1 3BA. U.K
+44(0)164 234 2428


________________________________________
From: mems-talk-bounces@memsnet.org [mems-talk-bounces@memsnet.org] On Behalf Of
闫许 [microyanxu@gmail.com]
Sent: 04 January 2010 01:47
To: mems-talk@memsnet.org
Subject: [mems-talk] Does petrol swell or etch PDMS?

Dear all,

       I would like to protect my chip immerged in petrol using PDMS film.
Does petrol swell or etch PDMS?

       Thanks a lot!

X. Yan
Shanghai Institute of Microsystem And Information Technology
reply