durusmail: mems-talk: protecting layer/material during KOH Si etching forSiN membrane formation
protecting layer/material during KOH SiN membrane formation
2010-01-07
protecting layer/material during KOH Si etching forSiN membrane formation
protecting layer/material during KOH Si etching forSiN membrane formation
Morrison, Richard H., Jr.
2010-01-12
You can use black wax Apiezon.

Rick


-----Original Message-----
From: mems-talk-bounces@memsnet.org
[mailto:mems-talk-bounces@memsnet.org] On Behalf Of Xiaoyong Liu
Sent: Thursday, January 07, 2010 3:08 PM
To: mems-talk@memsnet.org
Subject: [mems-talk] protecting layer/material during KOH Si etching
forSiN membrane formation

Hi All,

      I am in a processing of making SiN membrane by using KOH chemical
etching on SiN(~50nm) coated Si wafers. There are some patterns on one
side of wafer, and I want them intact during KOH etching. The total
etching time will be about 5-6 hours.  I am wondering if there is any
material/film I can put on to protect that side of wafer, and can be
readily removed afterwards.

Thanks a lot

Xiaoyong
reply