Hi everybody,

I want to do dry etching of GaAs with Gold as a mask since my special process
flow. But as I know, Gold will be etched in the Cl2, which is necessary for GaAs
etching.

Can anybody give me a proper recipe for this process?

Many thanks.

Regards,
Terry