Dear Harshal, had you checked the temperature during UV exposure, high temperature may "bake" / stick the tape to your wafer. How about UV dosis, meassured in mJ/cm², only exposure time is not enough information. If UV dosis is too high, higher than required, tape can also stick to your waver. Best regards Matthias