I used the ratio of 10:1 by volume and no difference was found. > -----Original Message----- > From: DEBASHIS MAJI> Date: Tue, 9 Mar 2010 00:54:57 +0530 > To: General MEMS discussion > Subject: [mems-talk] PDMS mixing > Dear all, > > I have a small question regarding mixing up of the PDMS base and the hardner > in 10: 1 ratio. Generally it is specified as mixing up of the two in 10:1 > ratio by weight. But can anyone tell me whether their will be a lot of > difference in the PDMS property if one use the ratio of 10:1 by volume ( eg. > 10ml : 1ml ). Normally we can correlate the weight ratio to volume ratio, > but in that case can anyone please tell me the density of the base and > the hardner ? The density of the PDMS is about 0.97 kg/m3 . > > Thanks in advance. > > Debashis Maji,