Hi Darren, indeed, your lithography looks ...hm... not good. I'll guess, no lift-off possible. Something is really wrong with your litho. It could be: mask not in contact with substrate or wrong focus. Too low dosis (looking at 10um line). Old or contaminated resist/developer. Wrong processing order? Try to check this first with other users. 10um lines should be very easy to pattern. Furthermore, what is you substrate? Could it be that your (alkaline) developer attacked the substrate? Best Daniel -----Original Message----- From: mems-talk-bounces+d.grimm=ifw-dresden.de@memsnet.org [mailto:mems-talk-bounces+d.grimm=ifw-dresden.de@memsnet.org] On Behalf Of Darren Alvares Sent: Montag, 16. August 2010 02:12 To: mems-talk@memsnet.org Subject: [mems-talk] Lift Off Hi All, I am using a photoplotted transparency mask to pattern resist for a lift off process. I have a series of lines I have exposed. See image: http://yfrog.com/mhimage31np Looking at the pattern under the microscope indicates that there is no sharp edge on the corner. I have used AZ6632 positive resist. To me this doesn't look like it will be successful with lift off. This lines are smallest to largest 10,20,30..um. Any suggestions or thoughts on: -Whether lift off will occur. -What could be the problem. Resist, Exposure Time, Baking, Proper Contact with substrate? Looking forward to hearing from you regarding this. Cheers, Darren