durusmail
:
mems-talk
:
SOI wafer price for diameter 200mm 1000pcs
SOI wafer price for diameter 200mm 1000pcs
2010-08-19
杜 彦召
SOI wafer price for diameter 200mm 1000pcs
杜 彦召
2010-08-19
Anybody knows what is the price for a diameter 200mm SOI wafer ? where i can buy it? thanks . Andrew
reply