In our wafer processing we interchangeably use hard and vacuum contact lithography depending on the wafer geometry (and alignment tolerance). We have found that simply reducing the develop time, while maintaining all other parameters, results in a comparable process. So, why would a pattern exposed in hard contact develop faster than the same pattern in vacuum contact? Thanks, Zak Clark OptiComp Corp.