Ni adhesion to Si
Ni adhesion to Si
Ruiz, Marcos Daniel (SENCOE)
2010-09-14
You might try a Ti adhesion layer between the Ni and the Si

Dan

________________________________

From: mems-talk-bounces+dan.ruiz=3Dhoneywell.com@memsnet.org on behalf =
of Salam Gabran
Sent: Tue 9/14/10 9:52 AM
To: mems-talk@memsnet.org
Subject: [mems-talk] Ni adhesion to Si


Hi Guys,

I am trying to sputter deposit Ni on Si followed by annealing at a
different
temperature (350, 450 degreesC). The nickel is 30nm and 200nm.
During annealing, the Ni film peals off, it should be due to thermal
stresses during deposition.

Any clue how this can be resolved ?

kind regards

Salam R. Gabran, MASc.
Research associate, PhD. Candidate
Center for Integrated RF Engineering
(CIRFE) Group
ECE Dept., University of Waterloo