Rhistone from Dupont is one example. There are more suppliers. The PCB industry is using kilometers of these materials. -----Original Message----- From: mems-talk-bounces+shay=mizur.com@memsnet.org [mailto:mems-talk-bounces+shay=mizur.com@memsnet.org] On Behalf Of Mingke Xiong Sent: Wednesday, September 15, 2010 11:10 PM To: General MEMS discussion Subject: [mems-talk] Dry film photoresist for electroplating Hi guys, Does anyone know a good and cheap type of dry film photoresist that has good adhesion to PCB (Cu surface)? We want to use the PR mold for Zn/Sn plating. The minimum feature is about 50~60 um width straight lines. Thank you. Regards, Mingke Xiong AEM, Inc. 6610 Cobra Way San Diego, CA 92122, USA www.aem-usa.com 858-481-0210 (1660)