durusmail: mems-talk: copper plating
copper plating
2010-10-26
2010-10-27
2010-10-27
2010-10-28
2010-10-28
2010-10-27
2010-10-27
copper plating
Nabhiraj Yalagoud
2010-10-27
Hello MIngke,

May i know your application? I am wondering why you are plating Cu on Silver? as
such Silver would do the job of Cu even in a better way. Or is it to reduce
the cost of mass production ?

Nabhiraj


On Wed, Oct 27, 2010 at 8:30 PM, Mingke Xiong  wrote:

> Hi, dear Nabhiraj,
>
> Thank you for the advise. The current density needs to be reduced so that
> we can have a more uniform layer across the board.
>
> Regards,
>
> Mingke Xiong
reply