I know that s1813 sticks on SU-8 and 2000 if you use p20 adhesion promoter.
Cheers

-A

Also, is anyone else getting spam messages from Plamatherm with no way to
opt out of them?  I think they may have harvested my address from this
mailing list.

On Fri, Nov 5, 2010 at 12:01 PM, LEE  wrote:

> I am looking for a high selective solvent, which only remove shipley1813
> with no affect on AZ4620. Does anybody use it before?
>
> Btw, Does shipley 1813 stick well with SU-8?
>
> Thanks very much!
>
> LEE
reply