Hello Binh, Must the layer be Au/Ti only? If not, I think you can sputter Cr on your glass wafer first, then your desired layers. Cr offers a better adhesion on glass wafer. Hope this can help you. BR, YN WANG > Date: Thu, 2 Dec 2010 20:06:02 -0800 > From: binh_icd@yahoo.com > To: mems-talk@memsnet.org > Subject: [mems-talk] Au/Ti adhesion problem > > Hi all > > I'm having a problem with the Au/Ti adhesion on glass wafer as follow : > > I had finished the Au/Ti coating process on the glass wafer (piranha treated), there is no problem. Then I used some of them for my experiment at that time (the adhesion was good) and kept the others for the later use. > > After a few days when I used the others and there was a problem with the Au/Ti layer. They became sensitive and easily peel off even when washing with DI water. I don't know why there is a different adhesion between the first and the second time using. Does anyone face this problem before ? > > Thank you > > Binh Tran