Claude Beaulieu
1999-05-14
You can use "dry film". This is used in the PC board and flat pannel
display industries. The film is applied on the substrate by lamination.
Dupont is selling this type of material wich is a UV sensitive
negative resist.


At 10:45 AM 5/13/99 -0400, you wrote:
>
>Anyone know of something called photoresist "tape"?  Someone described it
>to me as being patternable photoresist, but in a "tape" solid form instead
>of that of liquid.  Please let me know where it can be purchased, and if
>such a product even exists.  Thanks.
>
>-Angela Rasmussen
>The George Washington University