Thin PMMA residual layer etch
2010-12-17
2010-12-20
Thin PMMA residual layer etch
Tsoll Doiiu
2010-12-20
I think you just should adjust plasma conditions, it works fine for etching of
residual even with 100nm patterns. However, for me it takes like a week of
playing with voltages and pressures (300mTorr, smth like 10V bias, don't
remember exactly)