Hi all. I just wanted to let you know that I did buy the SU-8 3005 and while the adhesion definitely is better on glass than the 2000 formulation, it is unfortunately not good enough. All patterns survive the development and look nice but they are not very well anchored to the surface. As I need them to stay there as permanent structures I would need to improve the adhesion a bit further. All wafers are still piranha cleaned and either singed or put through HMDS in a YES oven (since Microchem claims an improved adhesion with HMDS for the 3000 formulation). I've tried an HF-dip to clean and roughen up the surface but it didn't seem to improve anything. I've overexposed a wafer on purpose to make sure that it's not a matter of not cross-linking the layer closest to the glass surface, unfortunately no effect there either. What I have left to try, as far as I can think as least, is: - trying longer PEB times and doing very slow ramping (although I can't see any tendencies to cracking and my layer is really thin) - testing a couple of hours treatment in NaOH as I've read that it might help - try a plasma treatment of the wafer before putting it in the singe oven - try a silanization (APTMS/AEAPS) of the wafer before putting it in the singe oven If anyone has any other ideas/suggestions they are still very welcome :) best regards Mikael