Andrew Sarangan
2011-01-28
I should have added that I was talking about the older SU-2000 series
resist. The 3000 may behave differently.


On Fri, Jan 28, 2011 at 11:47 AM, Mikael Evander  wrote:
> So I'm not saying you are wrong, but I keep hearing this about the HMDS while
MicroChem keeps stating that it does help and have released a document with
measurements showing an almost 100% increase in adhesion for the 3000
formulation: http://www.microchem.com/products/pdf/SU-8-Adhesion-Results.pdf
>
> Is the general opinion that the data from Microchem can't be trusted, are
there other studies showing the opposite or why do people seem to ignore this?
>
> best regards
>
> Mikael
reply