Fahd, wet etching is probably the worst way of structuring PMMA. Why would you want to do it this way? You can mechanically mill, hot emboss, wire imprint, injection mold, laser ablate or laser cut PMMA and each of these methods is better than etching it. Cheers Holger -- Dr. Holger Becker microfluidic ChipShop GmbH Stockholmer Str. 20 D-07747 Jena Germany Geschäftsführerin: Dr. Claudia Gärtner Sitz der Gesellschaft: D-07745 Jena, Germany Amtsgericht Jena: HRB 209251 USt.-IdNr.: DE 221812444 -----Ursprüngliche Nachricht----- Von: mems-talk-bounces+hb=microfluidic-chipshop.com@memsnet.org [mailto:mems-talk-bounces+hb=microfluidic-chipshop.com@memsnet.org] Im Auftrag von Fahd Ali Gesendet: Dienstag, 10. Mai 2011 14:15 An: mems-talk@memsnet.org Betreff: [mems-talk] PMMA etching Hello everyone, I am using this service for the first time. I want to do wet etching of PMMA substrate. Does anyone have any idea how to do it. I want to make small channels in it. thanking you in advance. regards, Fahd