Hello Ali, You can try to increase the curing temperature appropriately. Best regards At 2011-05-26 10:34:51,"Ali M. Koupaei"wrote: >Hello all! > >I made PDMS on a patterned silicon master; however after cross-linking at 50oC overnight, the PDMS film cannot be removed from the master uniform and nicely; in fact the master is gone and PDMS can only be removed partially so much so no patterned PDMS can be achieved. > >Does anyone have any idea how I can solve this problem and what is wrong with the master? As usual I am using a 10:1 ratio of elastomer to cross-linker. For another master I do not have the same problem and PDMS film can be thoroughly removed from the master and nothing remains on master. > >Thanks a lot! >Ali