righeira carnegie
2011-05-27
hi,

   Usually, a release layer like FDTS Self assembled monolayer would be more
appropriate(10µl and SAM formation for 30mins will work) and 50° over night
will work after that, I did 70° overnight like this, yes it worked and is
very uniform. All the best.

Regards,
Righeira

On Thu, May 26, 2011 at 4:48 PM,  wrote:

> 50 C overnight is way too long. 65 for an hour is usually the time.
> Or RT if you leave it over night.
>
> Hope this helps.
>
> Petru