dicing problem with silicon wafer
Ruiz, Marcos Daniel (SENCOE)
2011-06-02
HF works with Si wafers because it removes the hydrophilic oxide. I would also
like to know how to do that with the Pt surfaces.
Dan
-----Original Message-----
From: mems-talk-bounces+dan.ruiz=honeywell.com@memsnet.org [mailto:mems-talk-
bounces+dan.ruiz=honeywell.com@memsnet.org] On Behalf Of Jie Zou
Sent: Thursday, June 02, 2011 8:54 AM
To: General MEMS discussion
Subject: Re: [mems-talk] dicing problem with silicon wafer
Doesn't HF do that for Si wafers? I don't know for the Pt surfaces.
Jie