Try contact the following company : EPOTECNY 10, impasse LATECOERE 78140 VELIZY, FRANCE Tel : +33 1 39 46 69 34 Fax : +33 1 39 46 70 03 They have different kinds of UV resines suitable for optical applications and others. ********************************************************* Dr. Kholdoun TORKI CMP-TIMA 46, Av. Felix Viallet, Kholdoun.Torki@imag.fr 38031 GRENOBLE, France. torki@rhin.imag.fr http://tima-cmp.imag.fr Fax : +33 4 76473814 Tel : +33 4 76574763 ********************************************************* prosegur wrote: > DEAR SIR , WE NEED TO KNOW ABOUT A RESIN TO BE USED IN THE BONDING OF > TWO LAYERS/LAMINATE OF GLASS( THICK:6MM EACH), > WITH UV RADIATION. > > BEST REGARDS prosegur@cantv.net or fafonso@cantv.net >