Eric Johnston
2011-06-10
Hi.

We spin coat then let the wafer rest for a day in a covered petri dish.
Then soft bake.

Eric

On Fri, Jun 10, 2011 at 12:07 PM, 첸로 wrote:

> Hello,
>
> I want to get a 120um thickness coating.