make the su-8 surface flat
Shane GUO
2011-06-13
Hi,

I agree with Eric. We also found that the relaxation time was very important to
us. We use SU-8 (50) and (25) for a 100um and 50um thick seed layer. However, we
did find that the SU-8 coating was pulled back from wafer edges after a long
relaxation. Did you find the same thing Eric? How to avoid that?


Regards