durusmail: mems-talk: Isotropic etching SiO2 with PMMA mask
Isotropic etching SiO2 with PMMA mask
Isotropic etching SiO2 with PMMA mask
Judith Linacero Blanco
2011-07-12
In fact,

When I etch the SiO2 with PMMA mask, I use the RIe (with CHF3and Ar). My
problem now is that the walls are not vertical and RIE only attacks in this
direction I have problems. How I can fix it?

Best regards,
reply