durusmail: mems-talk: Comments on manual wirebonders wanted
Comments on manual wirebonders wanted
1999-05-30
Comments on manual wirebonders wanted
Ken Westra
1999-05-30
We have an K and S manual wirebonder (model 4123) that we have been
using for the past 12 years. We find that it is very finicky machine to
use. A few people have the right touch and it works well, but for most
users it does not work well at all. It has always been this way.

  My question is: is this typical of manual wirebonders or is it a
problem with this particular machine that we can fix.

  Any comments on this problem or tricks for setting up the machine so
it works better are greatly appreciated.

  Thanks,

   Ken Westra
   Manager/Staff Scientist
   MicroFab at the University of Alberta


reply