Hello all,

We are using a pure CHF3 process to etch oxide for our process and our
roughing pumps are being damaged as a result. Small white flakes can
be found in the filter, which is also dyed red (from an initial beige
colour). Does anyone have any experience with this problem, and are
there any methods to over come it?

Regards,

-Geoff