Hi Gary, What did you mean 'expose the material properly'? Sorry to mention that the exposure dose is calculated by multiplying the time and intensity of 10 mJ/cm2. So, my exposure dose ranged from 70 mJ/cm2 to 100 mJ/cm2. Please comment either the dose is too low or too high. Thanks, Yingtao ________________________________________ From: mems-talk-bounces+y.tian2=lboro.ac.uk@memsnet.org [mems-talk- bounces+y.tian2=lboro.ac.uk@memsnet.org] On Behalf Of Gary Hillman [garyh@s-cubed.com] Sent: 10 January 2012 20:35 To: 'General MEMS discussion' Subject: Re: [mems-talk] SU-8 process development Sounds like you did not expose the material properly. Gary