Hello Ankita, Depending on the size of your chip, you may need a "Flip Chip Bonder". There can be slip and warping effects - especially if your die are on the order of 0.5 - 1 cm on an edge. Would be interested in knowing about your Au-Au pad size etc, as we are trying to do some work in Cu based bonding, and we are always looking for alternatives. Good Luck! John ________________________________ From: Ankita VermaTo: mems-talk@memsnet.org Sent: Monday, January 16, 2012 10:42 AM Subject: [mems-talk] Au-Au thermo-compression wafer bonding Hi Everyone, I would like to ask for some help regarding wafer bonding using Au-Au thin films. I have read many papers and know that plasma pretreatment will help in bonding wafers at lower temperatures (around 200 C). Though what my problem is that most of the papers that I have read state that the amount of pressure they used to bond these wafers using Au films was around 1-10MPa. This does not make sense for me as I do not have a flip chip bonder, and I am trying to bond wafers by just applying a weight on top of 2 wafers and then anneal them in a lab oven at 200 C. 1MPa = 145psi. For a 4 inch wafer it comes to 1822 pounds of weight required to bond them. This seems to be a lot of weight. I cannot bring so much weight to bond the wafers. Can anyone suggest a better way to try bonding the wafers? How can I try doing this experiment without having a flip chip bonder? Please help!! -- Best Regards Ankita Verma