Hi,

  What sort of electrical resistance between wafers can be achieved with
thiol bonding?



On Thu, Jan 19, 2012 at 6:51 AM, Felix Lu  wrote:

> Hi Ankita,
>
>     Electronic Visions and Suss and probably a few other companies make
> bonders. You might also consider looking for a hot isostatic press. These
> are usually found in mechanical engineering depts ( and online) - but you
> have to be careful  in your interaction with them -- their standards of
> "clean" (more or less spit on it and shine  the sample on their shirt...)
> are very different from those needed for wafer bonding!
>
> Good luck!
>
> Felix
>