etched glass
Fahd Ali
2012-12-04
Hi,

I have problem regarding glass etching. I made micro-channels using HF-40% on
glass wafers. The problem is I have very sharp edges, which is not surprising.
But for my application I need smooth edges.

Is there any way during etching or after ?
your answers are highly appreciated.

regards,
Fahad