durusmail: mems-talk: SU-8 2005 overexposed?
SU-8 2005 overexposed?
2013-01-17
2013-01-18
2013-01-18
2013-01-19
2013-01-19
2013-01-21
2013-01-21
2013-01-22
2013-02-04
2013-02-04
SU-8 2005 overexposed?
Bill Moffat
2013-02-04

Try a vacuum soft bake to assist in removing solvent.  Bill Moffat