Hi, Shane (et al), We purchased a very inexpensive spin coater (with vacuum chuck) from Delta Scientific Equipment Pvt. Ltd. India in Kolkata. It is a little less polished than more expensive systems but works fine. Jeff Prof. Jeffrey P. Wolinski Department of Physics Grove City College -----Original Message----- From: mems-talk-bounces+jpwolinski=gcc.edu@memsnet.org [mailto:mems-talk- bounces+jpwolinski=gcc.edu@memsnet.org] On Behalf Of Shane Sent: Saturday, July 20, 2013 11:54 AM To: mems-talk@memsnet.org Subject: [mems-talk] spin coater suppliers Hello all, Would you please also give me some suppliers for spin coater? I know Laurell is one of them. Do I have other options? Cheers Shane _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk _______________________________________________ Hosted by the MEMS and Nanotechnology Exchange, the country's leading provider of MEMS and Nanotechnology design and fabrication services. Visit us at http://www.mems-exchange.org Want to advertise to this community? See http://www.memsnet.org To unsubscribe: http://mail.mems-exchange.org/mailman/listinfo/mems-talk